Aluminium, 7075 Tube
This grade is a heat treatable alloy with high strength. For outdoor atmospheric environments corrosion protection is recommended. This alloy is used for Aerospace and Defence high stress applications.
| Chemical Composition (Weight %) |
|||||||||||||||||
| Si | Fe | Cu | Mn | Mg | Cr | Zn | Ti | Al | |||||||||
| Min | 1.2 | 2.1 | 0.18 | 5.1 | |||||||||||||
| Max | 0.40 | 0.50 | 2.0 | 0.30 | 2.9 | 0.28 | 6.1 | 0.20 | Bal | ||||||||
| Typical Mechanical Properties (Min) | ||||||||||
| Temper | Tensile Strength, MPa | Yield Strength 0.2%, MPa | Elongation % | |||||||
| O | 228 | 103 | 17 | |||||||
| T6 | 572 | 503 | 11 | |||||||
| T73 | 503 | 434 | 13 | |||||||
Related Specifications and Conditions
ASTM B210, AMSWW-T-700/7, AMS-QQ-A-200/11, AMS4154
Available Forms
Tube, plate
| Chemical Composition (Weight %) |
||||||||
| Min | Max | |||||||
| Si | 0.40 | |||||||
| Fe | 0.50 | |||||||
| Cu | 1.2 | 2.0 | ||||||
| Mn | 0.30 | |||||||
| Mg | 2.1 | 2.9 | ||||||
| Cr | 0.18 | 0.28 | ||||||
| Zn | 5.1 | 6.1 | ||||||
| Ti | 0.20 | |||||||
| Al | Bal | |||||||
| Typical Mechanical Properties (Min) | |||||||
| Temper O | |||||||
| Tensile Strength, MPa | 228 | ||||||
| Yield Strength 0.2%, MPa | 103 | ||||||
| Elongation % | 17 | ||||||
| T6 | |||||||
| Tensile Strength, MPa | 572 | ||||||
| Yield Strength 0.2%, MPa | 503 | ||||||
| Elongation % | 11 | ||||||
| T73 | |||||||
| Tensile Strength, MPa | 503 | ||||||
| Yield Strength 0.2%, MPa | 434 | ||||||
| Elongation % | 13 | ||||||
Related Specifications and Conditions
ASTM B210, AMSWW-T-700/7, AMS-QQ-A-200/11, AMS4154
Available Forms
Tube, plate